20Pcs Low Temperature Wire Brazing Solution Welding Flux-Cored Rods 2mm*50cm US

$ 6.11

Availability: 181 in stock
  • Welding Rod Material: Aluminum Alloy
  • Refund will be given as: Money back or replacement (buyer's choice)
  • Diameter: 2mm
  • Melting Point: 647℃~658℃
  • Condition: New
  • All returns accepted: Returns Accepted
  • Restocking Fee: No
  • MPN: Does Not Apply
  • Brand: Unbranded
  • Welding Rod Type: Flux Cored Welding Rod
  • Return shipping will be paid by: Buyer
  • Item must be returned within: 30 Days
  • Length: 50c'm
  • Quantity: 20pcs/50pcs

    Description

    20Pcs Low Temperature Wire Brazing Solution Welding Flux-Cored Rods 2mm*50cm US
    Features:
    1. Great Welding Effect - With full & smooth welding effect because of internal powder.
    2. With low melting point(647℃~658℃), great weldability and corrosion resistance, high thermal conductivity, high electric conductivity and excellent processing performance.
    3. No Need Solder Powder - You don't have to use other flux powder with aluminum alloy as the welding core and coating as the salt base. Very convenient and easy to weld.
    4. Widely Use In Life - Suitable for welding or surfacing welding alloy with high strength, good forgeability & good corrosion resistance.
    5. Very Wide Application -  It is mainly used for argon arc welding and filling material for pure aluminum, connection with aluminium bus and guide rod of electrolytic aluminium plant and electric power, chemistry, food and so on.
    6. Light Weight & Small Volume,very easy to bend & carry.
    Specification:
    Quantity: 20PCS
    Material: Aluminum Alloy
    Color: Silver
    Melting Point: 647℃~658℃
    Diameter: 2mm / 0.08"
    Length: 500mm / 19.7"
    How to Use:
    Step 1: Clean and polishe the physical surface.
    Step 2: Heat the surface of the base material, until the temperature of the wire to the operating temperature of 380℃~400℃, so you can rely on the parent metal heat transfer welding wire to form welds, should not use the flame to burn wire, When the surface temperature of the base metal is sufficient, the wire can flow well and penetrate into the metal capillary.
    Step 3: When repairing thin aluminum, as long as the aluminum base metal heated to the appropriate working temperature, and then use the wire back and forth friction melting to form a weld, only with a metal brush melt welding wire to weld at the weld.
    Step 4: Use propane gas to weld s mall object, use industrial gas or induction heating device to heat and weld big object, natural slow cooling after welding.
    Application in Life:
    Can be used for a variety of heat sources, such as propane, oxy acetylene and so on. Low-temperature aluminum welding wire can weld almost all white metal, including aluminum, aluminum, cast aluminum, aluminum alloy and dissimilar welding between the above-mentioned metals, even for serious corrosion or oil pollution of white metal, and even that the aluminium alloy that cannot be repaired can be repaired. Applicable to the primary welding operator all-round welding, only a small heating device, after welding the weld strength is generally higher than the strength of the base metal itself, can understand the gas welding operation.
    NOTE:
    1. The surface of the base metal must be clean.
    2. The base metal temperature to reach 400 degrees, including the process of welding the base metal temperature should be maintained at 400℃, and the temperature can be high or low.
    Package Includes:
    20PCS* Aluminum Welding Wire
    We only accept the payment by Paypal.
    Buyers are required to carefully follow payment instructions on the checkout page, and note down any necessary details on it (e.g. bank account details).
    If buyers fail to follow the instructions on the checkout page, We are not liable for any unidentified payments and subsequent delivery delays.
    Shipment is within USA.
    Items are generally dispatched with
    in 1 working day after payment is cleared.
    Items will only be delivered during normal working hours
    (9am to 5pm on weekdays. Delivery is not available on weekends, public holidays or after business hours.
    Buyers will also be able to trace deliveries online with a unique tracking number. While we endeavor to send all our items with tracking numbers, there may be a few smaller items that are not sent with a tracking number.
    Buyers have full responsibility to provide us with the correct delivery address on the checkout page before payment is made.
    Re-delivery fee may be charged to buyers for items that are undelivered and/or returned to us due to incorrect delivery address or unsuccessful deliveries.
    If it is the buyer's personal reason to return the item ,the return postage fee would be at buyer's charge. Plus, the buyer also need to pay 10% restocking fee.
    Returns must be agreed by both parties prior to the actual return with 30 business days.
    Buyers must also strictly follow our returns procedure when returning an item.
    We reserves the rights to provide buyers a replacement, parts or a full or partial refund. Charges may apply if the product is damaged by buyers when the returned item is received.
    Should you change your mind and wish to return your item, this can be done if you notify us within 14 days of receiving your item. Please note, to qualify for such a return:
    - Please wait for our confirmation on how the item is to be returned.
    - The item must retain all original internal and external packaging.
    - The item itself must not be opened. We acknowledge the external box may have been opened for a visual inspection, but nothing else must be opened or used.
    - Just prior to returning it to us, ensure that there is nothing (e.g. return paperwork, email copy) stuck on the item or anywhere else inside of the box.
    - Any postage labels or return paperwork must be stuck on the outside box.
    Once the item has been returned, we will need to deduct the initial dispatch and also the return freight charges from your refund.
    Refunds will only be processed PayPal,  depending on the original method of payment.
    On Feb-21-20 at 07:25:46 PST, seller added the following information: